ONH836 Analyser

Determination of Oxygen, Nitrogen and Hydrogen in Steel, Refractory Metals and other Inorganic Materials.
 
Specifications
 
Measurement range for 1 g of sample
  • Oxygen 0.00005 to 50 mg
  • Nitrogen 0.00005 to 30 mg
  • Hydrogen 0.0001 to 2.5mg
  •  
    Sample images are shown here:
     

  • Sample required for light alloys:1gram
  • Sample dimension: pins 2-3mm dia and
    6-9 mm length
  • Sample required for
    heavy alloys:0.1gram powder
  •  
     
     
     
     
    For heavy alloys (Ti/W/Mo) samples will be weighed using Tin capsules and inserted in Nickel baskets and then placed in graphite crucibles containing graphite powder and subjected to combustion. Nickel baskets and Graphite powder are used as accelerators.
     
  • Sample preparation: According to ASTM procedure
  • Crucible available: Graphite
  • Software: Cornerstone

ONH836

Maximum 5 samples will be accepted for each workorder..

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 
   
   
 